Nickel Felt Roll (1000mm L x 200 mm W x 0.45 mm T) as Conductive Substrate for Flow Battery, Fuel Cells, and Electrolyzer - EQ-bcnf-045m
HomeStore

Nickel Felt Roll (1000mm L x 200 mm W x 0.45 mm T) as Conductive Substrate for Flow Battery, Fuel Cells, and Electrolyzer - EQ-bcnf-045m

Nickel Felt Roll (1000mm L x 200 mm W x 0.45 mm T) as Conductive Substrate for Flow Battery, Fuel Cells, and Electrolyzer - EQ-bcnf-045m

$489.64

Original: $1,398.96

-65%
Nickel Felt Roll (1000mm L x 200 mm W x 0.45 mm T) as Conductive Substrate for Flow Battery, Fuel Cells, and Electrolyzer - EQ-bcnf-045m

$1,398.96

$489.64

The Story

 Specifications

  • Material: Nickel Felt Roll, Purity> 99.99% (excellent anti-corrosive)
  • Dimension/Property: 
    • Length:  1000 mm 
    • Width:     200mm
    • Thickness:   0.45 mm
    • Porosity: 82%
  • Notice: Please notice that it is normal to observe NiO peaks in the nickel foam in XRD data. It is really difficult to avoid the oxidation of the nickel.
  • How to clean the Nickel Foam for Battery Cathode Substrate.  
  1. It can be removed from the NiO by annealing in the hydrogen furnace.
  2. Nickel fel sheet can be carefully cleaned with the concentrated HCl solution (37 wt.%) in an ultrasound bath for 5 min in order to remove the surface oxide layer. And then deionized water and absolute ethanol were used for 5 min each to ensure the surface of the Ni foam was well cleaned. 




Nickel Felt Roll (1000mm L x 200 mm W x 0.45 mm T) as Conductive Substrate for Flow Battery, Fuel Cells, and Electrolyzer - EQ-bcnf-045m - Image 2

Details & Craftsmanship

Every detail has been carefully considered to bring you the perfect product.

Description

 Specifications

  • Material: Nickel Felt Roll, Purity> 99.99% (excellent anti-corrosive)
  • Dimension/Property: 
    • Length:  1000 mm 
    • Width:     200mm
    • Thickness:   0.45 mm
    • Porosity: 82%
  • Notice: Please notice that it is normal to observe NiO peaks in the nickel foam in XRD data. It is really difficult to avoid the oxidation of the nickel.
  • How to clean the Nickel Foam for Battery Cathode Substrate.  
  1. It can be removed from the NiO by annealing in the hydrogen furnace.
  2. Nickel fel sheet can be carefully cleaned with the concentrated HCl solution (37 wt.%) in an ultrasound bath for 5 min in order to remove the surface oxide layer. And then deionized water and absolute ethanol were used for 5 min each to ensure the surface of the Ni foam was well cleaned.